In contrast, Nuruddin et al. applied ball milling after chemical treatments. 52 The cellulose used as a starting material in this case was extracted from wheat straw and kenaf fibers via formic acid/peroxyacetic acid and hydrogen peroxide treatment. Milling was then performed in 80% ethanol for 30–120 minutes using a highenergy ball mill.