Mar 08, 2015 · Mar 08, 2015 · Cleaning Powder gold of nitric acid. Powder gold boiled with clean water for 1015 minutes, temperatures 7090 0 C Pour the water out. This is dry gold dregs. When the water dries out, slowly pour the gold powder into a crucible (or the AR process to be more gold purity> 99%) Given some heat to gold power but use low heater.