Abstract: Welded arc welding repair welding technology was used to repair the casting defects of high chromium cast iron ball mill liners. Select the same highchromium cast iron as the casting. The diameter of the electrode is 4mm and the welding current is 150160A. After welding, the castings were found to have no cracks by surface non ...